ESAB |
技術(shù)標(biāo)準(zhǔn) |
熔敷金屬力學(xué)性能 |
熔敷金屬化學(xué)成分(%) |
|||||||||
SFA/AWS |
EN |
屈服值 Mpa |
抗拉強(qiáng)度 Mpa |
延伸率% |
沖擊值 |
C |
Si |
Mn |
Ni |
Cr |
Mo |
||
手工焊條 |
OK 48.08 |
A5.5-96 E7018-G |
EN 499 |
540 |
600 |
26 |
-20 ℃ 160 |
0.06 |
0.35 |
1.2 |
0.9 |
- |
- |
OK 73.15 |
A5.5 |
EN 499 |
550 |
610 |
28 |
-50 ℃ 120 |
0.06 |
0.4 |
1.4 |
0.9 |
- |
- |
|
OK 73.68 |
A5.5 |
EN 499 |
520 |
610 |
26 |
-55 ℃ 110 |
0.05 |
0.35 |
1.0 |
2.4 |
- |
- |
|
OK 73.79 |
A5.5 |
EN 499 |
520 |
610 |
26 |
-60 ℃ 160 |
0.06 |
0.3 |
0.6 |
3.3 |
- |
- |
|
OK 74.46 |
A5.5 |
EN 1599 |
460 |
560 |
27 |
+20 ℃ 175 |
0.06 |
0.3 |
0.8 |
- |
- |
0.5 |
|
OK 74.70 |
A5.5 |
EN 499 |
540 |
630 |
26 |
-20 ℃ 110 |
0.08 |
0.4 |
1.5 |
- |
- |
0.4 |
|
OK 74.78 |
A5.5 |
EN 1599 |
600 |
650 |
24 |
0 ℃ 100 |
0.06 |
0.35 |
1.5 |
- |
- |
0.35 |
|
OK 75.75 |
A5.5 E11018-G |
EN 757 |
755 |
820 |
20 |
-20 ℃ 85 |
0.05 |
0.35 |
1.75 |
2.25 |
0.45 |
0.45 |
|
OK 75.78 |
|
EN757 E89 6 Mn3NiCrMo B 42 H5 |
920 |
965 |
17 |
-60 ℃ 60 |
0.05 |
0.3 |
2.1 |
3.1 |
0.5 |
0.6 |
|
OK 76.18 |
A5.5 E8018-B2 |
EN 1599 |
530 |
620 |
20 |
+20 ℃ 120 |
0.06 |
0.3 |
0.7 |
- |
1.3 |
0.5 |
|
OK 76.28 |
A5.5 |
EN 1599 |
550 |
650 |
18 |
+20 ℃ 120 |
0.06 |
0.3 |
0.7 |
- |
2.3 |
1.1 |
|
OK76.35 |
A5.5 |
EN 1599 |
/ |
460 |
35 |
+20 ℃ 145 |
0.05 |
0.4 |
0.7 |
- |
5.0 |
0.55 |
|
OK 76.96 |
A5.5 E8015-B8 |
EN 1599 E CrMo 9 B |
/ |
> 450 |
> 20 |
+20 ℃> 80 |
0.05 |
0.5 |
0.8 |
- |
9.5 |
1.0 |
|
OK 78.16 |
A5.5 E9018-G |
|
870 |
900 |
18 |
+20 ℃ 50 |
0.18 |
0.4 |
0.8 |
- |
1.0 |
0.2 |