Grade : | Z8C12 耐腐蝕鋼片/板和帶材 | ||||
Number: | X6Cr13 | ||||
Classification: | 鐵素體不銹鋼 | ||||
Density: | 7.7 g/cm 3 | ||||
Standard: | EN 10088-2:2005不銹鋼。通用耐腐蝕鋼片/板和帶材交貨技術(shù)條件 | ||||
EN 10088-3:2005不銹鋼。一般用途耐腐蝕鋼的半成品、棒材、線材、型材和光亮產(chǎn)品的交貨技術(shù)條件 | |||||
EN 10088-1:2005不銹鋼。不銹鋼清單 | |||||
Equivalent grades: | |||||
Chemical comb % of steel X6Cr13 (Z8C12 ): EN 10088-2-2005 | |||||
未經(jīng)買方同意,不得故意將本表中未列出的元素添加到鋼材中,除非對(duì)鑄件進(jìn)行精加工。 | |||||
特定的硫含量范圍可以改善特定的財(cái)產(chǎn)。對(duì)于可加工性,建議并允許將硫含量控制在0.015%至0.030%之間。對(duì)于可焊性,建議并允許將硫含量控制在0.008%至0.030%之間。對(duì)于可極化性,建議將硫含量控制在最大0.015%。 | |||||
C | Si | Mn | P | S | Cr |
max 0.08 | max 1 | max 1 | max 0.04 | max 0.015 | 12月14日 |
Mechanical properties of steel X6Cr13 (Z8C12 ) | |||||
Rm - Tensile strength (MPa) (+A) | 400-600 | ||||
Rp0.2 0.2% proof strength (MPa) (+A) | 220-240 | ||||
A - Min. elongation at fracture (%) (+A) | 19 | ||||
Brinell hardness (HB): (+A) | 200 | ||||
Properties of steel X6Cr13 (Z8C12 ) | |||||
Resistance to intergranular corrosion: in the delivery condition - no; in the welded condition - no |