分類: | E7015-B2L, SFA/AWS A5.5, E CrMo1L B 2 2 H5, EN ISO 3580-A |
認(rèn)證: | C1M-Low C, BV, 03919, VdTüV |
Approvals are based on factory b. Please contact ESAB for more inbation.
Alloy Type: | Low alloyed |
Coating Type: | Basic |
Diffusible Hydrogen: | <5.0 ml/100g |
Welding Current: | DC+ |
Testing Temperature |
ISO PWHT 690°C 1h |
20 °C |
ISO PWHT 690°C 1h |
AWS PWHT 690°C 1h |
Fusion time per electrode at 90% I max | kg weld bl/kg electrodes | Number of electrodes/kg weld bl | 安培 | 熔敷率 | 電壓 V | 直徑 |
63 hr | 0.59 kg | 76.9 | 65-95 A | 0.7 kg/h | 24 V | 2.5 x 350 mm |
70 hr | 0.56 kg | 50.0 | 90-130 A | 1.0 kg/h | 24 V | 3.2 x 350 mm |
80 hr | 0.59 kg | 33.3 | 125-165 A | 1.3 kg/h | 24 V |
4.0 x 350 mm |